Difference Between Inconel 600 and 625 Chemical Composition
Inconel 600 Chemical Composition
Inconel 625 Chemical Composition
Compare Inconel 600 vs 625 Price Per Kg
Concerning the Latest Inconel 600 vs. Inconel 625 Price List Contact Us Reach Out to Us Speak with us to receive a quote right away.
| Inconel 600 |
Price in USD |
Price in INR |
| Pipe |
$ 46 |
₹ 3852 |
| Sheet |
$ 45 |
₹ 3768 |
| Fasteners |
$ 48 |
₹ 4019 |
| Plate |
$ 44 |
₹ 3684 |
| Pipe Fittings |
$ 46 |
₹ 3852 |
| Forged Fittings |
$ 47 |
₹ 3935 |
| Round Far |
$ 47 |
₹ 3935 |
| Flanges |
$ 48 |
₹ 4019 |
| Inconel 625 |
Price in USD |
Price in INR |
| Pipe |
$ 46 |
₹ 3852 |
| Sheet |
$ 45 |
₹ 3768 |
| Fasteners |
$ 48 |
₹ 4019 |
| Plate |
$ 47 |
₹ 3935 |
| Pipe Fitting |
$ 46 |
₹ 3852 |
| Forge Fitting |
$ 44 |
₹ 3684 |
| Round Bar |
$ 47 |
₹ 3935 |
| Flanges |
$ 48 |
₹ 4019 |
Know Alloy 600 and 625 Differ With Each Other Application Wise
Alloy 600 and 625 Difference Application Wise
| Alloy
600 |
Alloy 625 |
| Automotive |
Aerospace |
| Thermal Processing |
Power Generation |
| Electrical Resistance |
Oil and Gas |
| Chemical Processing |
Chemical Processing |
| Welding Products |
Welding Products |
Understand Comparison Between UNS N06600 and N06625 Material Based On Corrosion Resistance
Comparison Between UNS N06600 and N06625 Corrosion Resistance
| Property |
Inconel 600 |
Inconel 625 |
| Oxidation Resistance |
Up to 1093°C |
Superior for thermal cycling |
| Extreme Environments |
Dry, High Temp |
Harsh, Variable |
| Chloride-Ion Environments |
Good |
Excellent |
| Pitting & Crevice Corrosion |
Moderate |
Superior |
| Acidic Conditions |
Good |
Excellent |
| Alkaline Conditions |
Highly Effective |
Effective |
| Applications |
Heat Exchangers |
Marine, Aerospace |
Find Key Differences Between WNR 2.4816 and 2.4856 Related to Fabrication and Heat Treatment
Differences Between WNR 2.4816 and 2.4856 Fabrication and Heat Treatment
| Property |
Inconel 600 |
Inconel 625 |
| Welding |
special techniques |
Easier |
| Fabrication |
Accurate temperature regulation is necessary. |
Easier to fabricate |
| Workability |
Work-intensive, hot/cold workable |
Quick hardening |
| Heat Treatment |
1600°F |
2,100 to 1,650°F |
Alloy 600 Vs Alloy 625 Standards
Inconel 600 vs Inconel 625 Physical Properties
| Physical Properties |
Inconel 600 |
Inconel 625 |
| Density, lb/in.³ |
0.306 |
0.305 |
| Density, g/cm³ |
8.47 |
8.44 |
| Melting Range, °C |
1354-1413 |
1290-1350 |
| Melting Range, °F |
2470-2575 |
2350-2460 |
| Curie Temperature, °F |
-192 |
<-320 |
| Permeability at 200 oersted |
1.010 |
1.0006 |
| Curie Temperature, °C |
-124 |
-196 |
| 625 Inconel Alloy |
| Density |
8.44 g/cm³ |
| 625 Alloy |
| Hardness |
22 HRC |
Temperature of Inconel 600 and Inconel 625
Inconel 600
- Temperature Limit: Up to 2000°F (1093°C)
- Applications: Heat exchangers, furnace components
Inconel 625
- Temperature Limit: Recommended up to 1200°F (649°C)
- Applications: Aerospace, power generation components